Image:Tough A96.JPG

From Wikipedia, the free encyclopedia

[edit] Summary

Description

Vickers toughness indention (P = 10 kg) in the microstructure of unetched 96% Al2O3 ceramic modulus-of-rupture bar in reflected light.

Source

self-made

Date

22:36, 8 January 2008 (UTC)

Author

His Manliness (talk)

Permission
(Reusing this image)

none required.

Other versions none.

[edit] Licensing


I, the copyright holder of this work, hereby publish it under the following licenses:
You may select the license of your choice.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeDimensionsUserComment
current22:36, 8 January 20084,032×3,104 (1.45 MB)His Manliness (Talk | contribs) ({{Information |Description = Vickers toughness indention (P = 10 kg) in the microstructure of unetched 96% Al2O3 ceramic modulus-of-rupture bar in reflected light. |Source = self-made |Date = ~~~~~ |Author = His Manliness ([[User t)

The following pages on the English Wikipedia link to this file (pages on other projects are not listed):